Abstract
The method is based on preparation of discs by incorporating the test portion of the iron ore sample via fusion into a borate glass disc using a casting procedure (using lithium borate or sodium borate as the flux). It has been designed to cope with iron ores having high ignition losses, using loss-corrected matrix coefficients. X-ray fluorescence measurements of the discs are based on the "line only" principle. Informative Annex H gives computer programs for calculation of the results.
General information
-
Status: WithdrawnPublication date: 1992-10Stage: Withdrawal of International Standard [95.99]
-
Edition: 1Number of pages: 71
-
Technical Committee :ISO/TC 102/SC 2ICS :73.060.10