Abstract
The principle of the test method specified is subjecting a test piece to uniaxial tensile strain at a prescribed constant rate within the region of uniform plastic strain. It is valid only for that part of the stress-strain curve in the plastic range where the curve is continuous and monotonic. The tensile strain hardening exponent is calculated either by considering a portion of the stress-strain curve in the plastic strain region, or by considering the whole of the uniform plastic strain region.
General information
-
Status: WithdrawnPublication date: 1993-02Stage: Withdrawal of International Standard [95.99]
-
Edition: 1Number of pages: 5
-
Technical Committee :ISO/TC 164/SC 2ICS :77.040.10